Repository logo
 

Electrical properties of kaolinite

Loading...
Thumbnail Image

Date

1969

Journal Title

Journal ISSN

Volume Title

Publisher

Te Herenga Waka—Victoria University of Wellington

Abstract

Asymmetric potentials are produced on heating a kaolinite sample held between platinum electrodes. Under vacuum the potentials rise to a peak of about 500 mV at about 500°C and under atmospheric pressure a peak of about 120 mV at about 600°C. The potential peak at 500°C is reproduced at about 575°C on cooling and reheating under vacuum conditions. The potential peak is dependent on heating rate to a marked degree; a slower heating rate of around 5°C/min produced no peak at 500 - 700°C but did produce a peak that is stable for a week at 800°C of about 800 mV. while a faster rate of around 30° C/min introduces further peaks. The potentials under vacuum at a heating rate of 10°C/min are shown to agree well with a calculated curve based on dehydroxylation of material at one electrode in preference to the material at the other electrode, such that where E is the potential produced, U is the heat of transport for the conducting species plus the heat of formation of a defect, F is the Faraday constant,ρ and σ are the density and thermal conductivity of the material, ΔH is the enthalpy of the reaction,Ap and Ep are the Arrhenius parameters R is the gas constant and α is the fraction of material which has reacted. The other potential curves are interpreted in terms of this equation. A study of oxygen loss from a metakaolinite sample was negative.

Description

Keywords

Electrochemical analysis, Kaolinite, Chemistry

Citation

Collections